— Troubleshooting guide

E6013 Welding Problems & Solutions: The Complete Troubleshooting Guide

E6013 is India’s most popular general-purpose welding electrode — easy to strike, smooth to run and forgiving on mild steel. But even a good rod gives bad welds when the current, technique or storage is off. This guide lists the most common E6013 problems we hear from welders across India, what causes each one, and how to fix it on the shop floor.

Updated 2026-11-12

Recommended current for E6013 electrodes

Electrode sizeTypical current (AC/DC)Best for
2.5 mm60 – 90 AThin sheet (1.5–3 mm), gates, grills, furniture
3.15 mm90 – 130 AGeneral fabrication, 3–6 mm plate — the workshop all-rounder
4.0 mm130 – 180 AStructural steel, 6–12 mm plate, sheds and trusses
5.0 mm180 – 240 AHeavy sections, flat and horizontal fillets

Start in the middle of the range and adjust by 5–10 A at a time. Go lower for vertical-up and overhead positions, higher for flat fillets on thick plate.

1. Porosity (pinholes or gas bubbles in the weld)

  • Cause: damp electrodes — moisture in the flux coating turns into gas inside the weld pool.
  • Cause: rust, oil, paint or galvanising on the base metal.
  • Cause: very long arc length, or strong wind blowing the shielding gas away.
  • Fix: re-dry rods at 100–150°C for 1–2 hours and store them sealed. Grind the joint to bright metal. Hold a short arc (roughly equal to the core wire diameter) and shield the work from wind.

2. Excessive spatter

  • Cause: current too high, arc too long, or damp rods.
  • Fix: drop the current by 10 A, shorten the arc and keep a 10–20° drag angle. Good-quality E6013 rods such as WELDARC and CUTWELD are formulated for low spatter — if spatter stays high on correct settings, check rod storage.

3. Electrode sticking to the job

  • Cause: current too low, or the rod is dragged in too close when striking.
  • Fix: raise the current by 5–10 A, strike like a matchstick and lift slightly. If the rod sticks, twist and pull it off quickly — do not leave it shorted, it overheats the coating.

4. Undercut along the weld toe

  • Cause: current too high, travel too fast, or the wrong electrode angle.
  • Fix: reduce current, slow down and pause briefly at each edge of the weave so filler fills the groove you are melting.

5. Slag inclusion

  • Cause: slag from the previous pass not removed, or slag running ahead of the arc on downhill or flat work.
  • Fix: chip and wire-brush thoroughly between passes. Increase the travel angle so the arc stays ahead of the molten slag, and raise current slightly if the puddle is sluggish.

6. Poor penetration or weak fusion

  • Cause: current too low, travel too fast, or joint gap too tight. Note: E6013 is a soft, shallow-penetrating rod by design.
  • Fix: raise current, slow down and leave a 1.5–2 mm root gap on butt joints. For deep-penetration or heavy industrial repair, use a heavier-duty electrode such as HITKARI GOLD.

7. Cracking in or next to the weld

  • Cause: high-carbon or thick restrained steel cooling too fast, or a concave undersized bead.
  • Fix: pre-heat thick sections to 100–150°C, avoid quenching with water, and make slightly convex beads. For high-carbon or critical joints, switch to a low-hydrogen (E7018-type) electrode.

8. Flux coating cracks or falls off

  • Cause: rods overheated by too much current, bent electrodes, or rough handling and over-drying above recommended temperature.
  • Fix: stay within the current range for the rod size, don’t bend rods, and store cartons flat in a dry place.

Storage: the cheapest fix of all

Most E6013 problems in Indian workshops trace back to moisture, especially in the monsoon. Keep cartons sealed until use, store off the floor away from walls, and re-dry rods that have been exposed to humid air. A small rod oven pays for itself in saved rework within weeks.

Frequently asked questions

Why does my E6013 electrode keep sticking?

The current is usually too low for the rod diameter. Raise it by 5–10 A, strike like a match and keep a short but steady arc. Damp rods also stick more, so re-dry them at 100–150°C.

What amperage should I use for a 3.15 mm E6013 rod?

Typically 90–130 A. Start around 110 A for flat work on 3–6 mm mild steel and reduce for vertical or overhead positions.

Can E6013 be used on AC welding machines?

Yes. E6013 runs well on AC transformers as well as DC machines, which is why it is the most common rod for Indian workshops.

How do I stop porosity with E6013?

Use dry rods, clean the joint to bright metal, hold a short arc and shield the job from wind. Porosity almost always comes from moisture or surface contamination.

Need the right rod for your job?

Tell us your base metal, thickness and machine — we’ll recommend the electrode and settings.

— Get Started

Transform your welding experience
today.

Join thousands of satisfied customers who trust Prakash Electrodes for their welding solutions. Get in touch for pricing, samples, or bulk orders.